一种​纳米特​种​工程塑料​及其​制备​方法

源语言标题
(CN104927339) 一种​纳米特​种​工程塑料​及其​制备​方法
公开号/公开日
CN104927339 A 2015-09-23 [CN104927339] / 2015-09-23
申请号/申请日
2015CN-0406648 / 2015-07-13
发明人
LI MINGHUA;
申请人
JIN BAOLI TECHNOLOGY SUZHOU;
主分类号
IPC分类号
C08K-003/22C08K-003/28C08K-005/372C08K-005/523C08K-013/02C08L-027/06C08L-067/00C08L-067/02C08L-071/12C08L-077/06
摘要
(CN104927339) 本​发明​属于​工程塑料​领域,公开​了​一种​纳米特​种​工程塑料​及其​制备​方法,所​述​的​工程塑料​包括​聚​苯​醚​树脂​16-30​重量​份、聚​癸​二​酰​乙​二​胺​5-15​重量​份、聚​癸​二​酸​甘油酯​4-10​重量​份、聚氯乙烯​11-20​重量​份、聚​己二酸​丙二醇​酯​3-7​重量​份、硫​代​二​丙​酸​二月​桂​酯​4-8​重量​份、磷酸​三​异​丙基​苯​酯​2-5​重量​份、纳米​氮化​钛​3-6​重量​份、纳米​氧化钙​4-8​重量​份。本​发明​的​工程塑料​制备​方法​包括​下述​步骤:(1)将​本​发明​的​成分​进行​机械​搅拌​均匀,备用;(2)将​步骤(1)搅拌​均匀​后的​混合​工程塑料​材料​再用​双​螺杆​挤出​机​熔融​挤出​并​造粒​后,为​纳米特​种​工程塑料。本​发明​的​工程塑料​具有​抗压强度​高、弯曲​强度​高、耐热​性能​高的​特点,适合于​电气工程​领域​中的​工程塑料​使用。
地址
代理人
代理机构
;
优先权号
2015CN-0406648 2015-07-13
主权利要求
(CN104927339) 1. A nano-engineering plastic, characterized in, nano-engineering plastic comprising the following parts by weight of materials: 16 the polyphenylene ether resin-30 parts, Polymetaxylylene 5 ethylenediamine-15 parts, 4 polyglycerol sebacate-10 parts, 11 polyvinyl chloride-20 parts, Polyethylene propylene adipate 3-7 parts, Thiodipropionic acid dilauryl February 4-8 parts, Phosphate triphenyl triisopropylsilyacetylene 2-5 parts, 3 titanium nano-6 parts, 4 calcium oxide nano-8 parts.  3. A nano-engineering plastic preparation method, characterized in, nanoparticle production method comprising the steps of engineering plastics including: 16 the polyphenylene ether resin(1)-weight 30 copies of copies, polymetaxylylene 5 ethylenediamine-15 parts by weight, polyglycerol sebacate 4-10 parts by weight, polyvinyl chloride 11-20 parts by weight, polypropylene adipate 3-7 parts by weight, thiodipropionic acid dilauryl February 4-8 parts by weight, phosphoric acid triisopropylphenyl 2-5 parts by weight, 3 titanium nano-6 parts by weight, cao 4 nano-8 parts by weight, with a speed of 60 r/min-150 r/min with mechanical stirring, stirring evenly to, standby; Mixing step(2)(1) under stirring for homogenization of the material is then engineering plastic melt extrusion and pelletizing twin screw extruder, twin-screw extruder speed is 50-200 r/min, twin-screw extruder at a temperature of 150-240 Ć, after granulation, is in the nanometer-engineering plastic.
法律状态
(CN104927339) LEGAL DETAILS FOR CN104927339  Actual or expected expiration date=2035-07-13    Legal state=ALIVE    Status=PENDING     Event publication date=2015-07-13  Event code=CN/APP  Event indicator=Pos  Event type=Examination events  Application details  Application country=CN CN201510406648  Application date=2015-07-13  Standardized application number=2015CN-0406648     Event publication date=2015-09-23  Event code=CN/A  Event type=Examination events  Published application  Publication country=CN  Publication number=CN104927339  Publication stage Code=A  Publication date=2015-09-23  Standardized publication number=CN104927339     Event publication date=2015-09-23  Event code=CN/C06  Event indicator=Pos  Event type=Examination events  Publication    Event publication date=2015-10-21  Event code=CN/C10  Event type=Examination events  Request of examination as to substance
专利类型码
A
国别省市代码
若您需要申请原文,请登录。